Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Promyde" in Material Data Center leads to the following information:

Tradename: Promyde
Family: PA6
Producer: Nurel S.A
86 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Promyde® B15P PA6
Promyde® B15U PA6
Promyde® B20 P PA6
Promyde® B24 PA6
Promyde® B25 PA6
Promyde® B27 PA6
Promyde® B30 NC 100 PA6
Promyde® B30 P PA6
Promyde® B30 P MI PA6
Promyde® B30 P N PA6
Promyde® B30 P2 G10 PA6-GF10
Promyde® B30 P2 G10 MI PA6-GF10
Promyde® B30 P2 G15 PA6-GF15
Promyde® B30 P2 G15 MI PA6-GF15
Promyde® B30 P2 G20 PA6-GF20
Promyde® B30 P2 G20 U0 PA6-GF20
Promyde® B30 P2 G30 PA6-GF30
Promyde® B30 P2 G30 MI PA6-GF30
Promyde® B30 P2 G30 U0 PA6-GF30
Promyde® B30 P2 G35 PA6-GF35
Promyde® B30 P2 G40 PA6-GF40
Promyde® B30 P2 G40 MI PA6-GF40
Promyde® B30 P2 G45 MI PA6-GF45
Promyde® B30 P2 G50 PA6-GF50
Promyde® B30 P2 GB30 PA6-GS30
Promyde® B30 P2 GFC15 PA6-GF15
Promyde® B30 P2 GFC30 PA6-GX30
Promyde® B30 P2 HI PA6
Promyde® B30 P2 M30 PA6-MX30
Promyde® B30 P2 MI PA6
Promyde® B30 P2 U0 PA6
Promyde® B30 U PA6
Promyde® B33 PA6
Promyde® B33 L PA6
Promyde® B33 LN PA6
Promyde® B35 P PA6
Promyde® B36 PA6
Promyde® B36 L PA6
Promyde® B36 LN PA6
Promyde® B40 PA6
Promyde® B40 L PA6
Promyde® B40 LN PA6
Promyde® A30 P2 G30 PA66-GF30
Promyde® B30 P2 G20 MI PA6-GF20
Promyde® B30 P2 G25 WR PA6-GF25
Promyde® B30 P2 G45 PA6-GF45
Promyde® B30 P2 HI C PA6
Promyde® B30 P2 HI60 PA6
Promyde® B30 P2 U0 T PA6
Promyde® B33 BR1 PA6
Promyde® B40 BR1 PA6
Promyde® B40 P2 FLX HI PA6
Promyde® B40 P2 U0 PA6
Promyde® B50 L PA6
Promyde® B300 HF PA6
Promyde® B300 P PA6
Promyde® B300 P2 G15 MI PA6-GF15
Promyde® B300 P2 G15 PA6-GF15
Promyde® B300 P2 G20 U0 PA6-GF20
Promyde® B300 P2 G30 S PA6-GF30
Promyde® B300 P2 G30 U0 PA6-GF30
Promyde® B300 P2 G30 PA6-GF30
Promyde® B300 P2 G35 S PA6-GF35
Promyde® B300 P2 G35 PA6-GF35
Promyde® B300 P2 G40 S PA6-GF40
Promyde® B300 P2 G40 PA6-GF40
Promyde® B300 P2 G50 S PA6-GF50
Promyde® B300 P2 G50 PA6-GF50
Promyde® B300 P2 G60 S PA6-GF60
Promyde® B300 P2 G60 PA6-GF60
Promyde® B300 P2 GFC15 PA6-GF15
Promyde® B300 P2 HI60 PA6
Promyde® B300 P2 M40 PA6-MX40
Promyde® B730 P PA6
Promyde® B930 P PA*
Promyde® BF33 L PA6
Promyde® BF33 LN PA6
Promyde® BF36 L PA6
Promyde® BF36 LN PA6
Promyde® BF40 L PA6
Promyde® BF40 LN PA6
Promyde® BF640 PA*
Promyde® BF740 PA*
Promyde® BF933 PA*
Promyde® BF940L PA*
Promyde® BF940LN PA*

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.