Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Stylac - ABS, SAN - Asahi Kasei

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Stylac" in Material Data Center leads to the following information:

Tradename: Stylac
Family: ABS, SAN
Producer: Asahi Kasei
48 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Stylac 026 ABS
Stylac 120 ABS
Stylac 121 ABS
Stylac 181 ABS
Stylac 183 ABS
Stylac 185 ABS
Stylac 190 ABS
Stylac 190F ABS
Stylac 191 ABS
Stylac 191F ABS
Stylac 220 ABS
Stylac 321 ABS
Stylac 767 SAN
Stylac 769 SAN
Stylac 783 SAN
Stylac 789 SAN
Stylac A100 ABS
Stylac A3921 ABS
Stylac A4130 ABS
Stylac AE490 ABS
Stylac AE510 ABS
Stylac AE850 ABS
Stylac CS747 SAN
Stylac FW130 ABS
Stylac FW920 ABS
Stylac IB330 ABS
Stylac IC10N ABS
Stylac IC24 ABS
Stylac IC39A ABS
Stylac ID31J ABS
Stylac ID510 ABS
Stylac IM10 ABS
Stylac IM15 ABS
Stylac IM20 ABS
Stylac IM30 ABS
Stylac IX220 ABS
Stylac IX600 ABS
Stylac IX700 ABS
Stylac NF920 ACS
Stylac R240A ABS-GF
Stylac R340T SAN-GF
Stylac R440T SAN-GF
Stylac T8701 SAN
Stylac T8707 SAN
Stylac VA518 ABS
Stylac VA58 ABS
Stylac VGB20 ABS-GF
Stylac VN33H ABS

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.