Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of TYMAX™ GT7001 - EMA - Westlake Chemical Corp.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Tymax datasheets, application examples or technical articles are available in Material Data Center
Extrusion coating
Laminations
Tie-layer
TYMAX® GT7001 is a maleic anhydride modified ethylene methyl acrylate copolymer designed for use as a tie layer in extrusion coating and lamination applications. This resin is designed for bonding to polyolefins, polyamides, and PET in multilayer film structures. It does not contain any slip or antiblock additives.
This product has some 21 CFR clearances.
Технологические и физические свойства | Значение | Единица | Стандарт | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Данные ASTM | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Показатель текучести расплава, ПТР | 6 | г/10 мин | ASTM D 1238 |
Теплофизические свойства | Значение | Единица | Стандарт | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Данные ASTM | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Температура плавления | 84 | °C | ASTM D 3418 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Температура размягчения по Вика | 51 | °C | ASTM D 1525 |
Прочие свойства | Значение | Единица | Стандарт |
Плотность | 942 | кг/м³ | ASTM D 792 |
Рекомендации по переработке экструзией | Значение | Единица | Стандарт |
Температура расплава | <330 | °C | - |
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.