Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Vampter - PBT - VAMP TECH SPA

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Vampter" in Material Data Center leads to the following information:

Tradename: Vampter
Family: PBT
Producer: VAMP TECH SPA
9 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Vampter 0023 V0 PBT
Vampter 1026 V0 PBT-GF10
Vampter 2026 V0 PBT-GF20
Vampter 3026 V0 PBT-GF30
Vampter 3028 V0 PBT-GF30
Vampter 4554 V0 60 F 20 PBT-(MX+GF)45
Vampter C 0023 V0 (PC+PBT)
Vampter C 3028 V0 (PC+PBT)-GF30
Vampter C 3528 V0 (PC+PBT)-GF35

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.