Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 47H BK0668 - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 47H BK0668:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Vydyne 47H BK0668 is general-purpose, medium impact-modified, heat stabilized PA66 resin. The product offers improved resistance to thermal degradation.
47H BK0668 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline.
Технологические и физические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Усадка при литье, продольная 1.8 / * % ISO 294-4, 2577
Усадка при литье, поперечная 1.6 / * % ISO 294-4, 2577
Механические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 2800 / 1700 МПа ISO 527
Напряжение в точке текучести 60 / 45 МПа ISO 527
Напряжение при разрыве 52 / 40 МПа ISO 527
Удлинение при разрыве 22 / 60 % ISO 527
Модуль упругости при изгибе, 23°C 2300 / 780 МПа ISO 178
Предел прочности при изгибе 70 / 24 МПа ISO 178
Ударная вязкость по Шарпи, +23°C N / N кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи, -30°C N / N кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи с надрезом, +23°C 16 / 62 кДж/м2 ISO 179/1eA
Ударная вязкость по Шарпи с надрезом, -30°C 11 / 24 кДж/м2 ISO 179/1eA
Ударная вязкость по Изоду образцов с надрезом, +23°C 18 / 44 кДж/м2 ISO 180/1A
Ударная вязкость по Изоду образцов с надрезом 16 / 24 кДж/м2 ISO 180/1A
Температура -30 °C -
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 260 / * °C ISO 11357-1/-3
Температура изгиба под нагрузкой, 1.80 МПа 63 / * °C ISO 75-1/-2
Температура изгиба под нагрузкой, 0.45 МПа 185 / * °C ISO 75-1/-2
Коэффициент линейного теплового расширения, продольный 110 / * E-6/K ISO 11359-1/-2
Коэффициент линейного теплового расширения, поперечный 140 / * E-6/K ISO 11359-1/-2
Класс горючести при номинальной толщине 1.5 мм HB / * класс IEC 60695-11-10
Толщина образца 1.5 / * мм -
Класс горючести при толщине образца h HB / * класс IEC 60695-11-10
Толщина образца 0.8 / * мм -
Glow Wire Flammability Index (GWFI) 700 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 мм -
Glow Wire Flammability Index (GWFI) 775 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 мм -
Glow Wire Flammability Index (GWFI) 700 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 мм -
Glow Wire Ignition Temperature (GWIT) 725 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 мм -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 мм -
Glow Wire Ignition Temperature (GWIT) 725 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 мм -
Данные ASTM
Класс огнестойкости (категория горючести) по стандарту UL 94 (ПВ-0) HB - UL 94
Толщина испытываемого образца 0.75 мм -
Электрические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Удельное объемное сопротивление 1E9 / - Ом*м IEC 62631-3-1
Электрическая прочность 12 / - кВ/мм IEC 60243-1
Сравнительный показатель пробоя 525 / - - IEC 60112
Данные ASTM
Сопротивление дуги 90 / - s ASTM D 495
Прочие свойствасухой / кондЕдиницаСтандарт
Водопоглощение 1.2 / * % Sim. to ISO 62
Поглощение влаги 2.3 / * % Sim. to ISO 62
Плотность 1100 / - кг/м³ ISO 1183
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 80 °C -
Время предварительной сушки 4 h -
Температура расплава 285 - 305 °C -
Температура формы 65 - 95 °C -
Зоны 1 280 - 310 °C -
Зоны 2 280 - 310 °C -
Зоны 3 280 - 310 °C -
Температура сопла 280 - 310 °C -
Особые свойства и характеристики
Способы переработки
Литье под давлением
Вид поставки
Гранулы, Черный
Особые показатели
Ударопрочный или модифицированный к удару, Термостабилизированный или стойкий к воздействию тепла
Химическая стойкость
Общая химическая стойкость, Стойкость к действию растворителей, Маслостойкость
Применение
Автомобилестроение, Электрические и электронные устройства, Общего назначения
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.