Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BMC 750 GRANITO - UP-(MD+GF)75 - Polynt S.p.A.

Material Data Center offers the following functions for BMC 750 GRANITO:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other BMC datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Soluble or severely attacked after brief contact.

Please consider the information about the application of the materials.
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Усадка при литье, продольная 0.1 % ISO 294-4, 2577
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Ударная прочность по Шарпи, +23°C 15 кДж/м2 ISO 179/1eU
Твердость по Роквеллу M 85 - ISO 2039-2
Other Standards[S]
Модуль упругости при изгибе, 23°C 11000 МПа ISO 14125A
Предел прочности при изгибе 60 МПа ISO 14125A
S: These properties are reported by the producer according standards that are different to our defaults.
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Сравнительный показатель пробоя 600 - IEC 60112
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 0.2 % Sim. to ISO 62
Плотность 1900 кг/м³ ISO 1183
Особые свойства и характеристики
Способы переработки
Прессование
Вид поставки
Формование в массе
Специальные характеристики
Сопротивление царапанию
Доступность материала по регионам
Европа
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.