Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Flomat 550/35 - UP-GF35 - Devi Polymers Private Limited

Material Data Center offers the following functions for Flomat 550/35:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flomat datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Other Standards[S]
Усадка при литье, продольная 0.2 % BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Механические свойстваЗначениеЕдиницаСтандарт
Other Standards[S]
предел прочности при растяжении 88 МПа BS-2782
Предел прочности при изгибе 186 МПа BS-2782
Прочность на сжатие 206 МПа BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Класс огнестойкости (категория горючести) по стандарту UL 94 (ПВ-0) V-0 - UL 94
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Сопротивление дуги 180 s ASTM D 495
Other Standards[S]
Удельное объемное сопротивление 1E12 Ом*м DIN 53482
Удельное поверхностное сопротивление 1E12 Ом DIN 53482
Электрическая прочность 11 кВ/мм BS 2782
S: These properties are reported by the producer according standards that are different to our defaults.
Прочие свойстваЗначениеЕдиницаСтандарт
Other Standards[S]
Водопоглощение 0.25 % BS-2782
Плотность 1800 кг/м³ BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Особые свойства и характеристики
Способы переработки
Прессование
Вид поставки
Полиэфирный листовой прессматериал
Доступность материала по регионам
Страны Азии и Тихого океана
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.