Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® PPA 5300 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® PPA 5300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® PPA 5300 resin is specially designed pellet used as a polymer process aid (PPA) for polyolefins.
 
The use of Kynar Flex® PPA 5300 resin at 200 - 1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control.

This product is also available on a powder form as Kynar Flex® PPA 5301 resin.
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 165 °C ISO 11357-1/-3
Прочие свойстваЗначениеЕдиницаСтандарт
Плотность 700 кг/м³ ISO 1183
Особые свойства и характеристики
Способы переработки
Пленочная экструзия, Экструзия листа, Экструзия (прочие виды)
Вид поставки
Мелкие гранулы, Порошок
Специальные характеристики
Сополимер
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Латинская Америка, Ближний Восток и Африка
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.