Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUTENE XL8080UCS - PE - LG Chem

Material Data Center offers the following functions for LUTENE XL8080UCS:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lutene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Механические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Предел прочности на разрыв 19.7 МПа ASTM D 638
Относительное удлинение при разрыве 500 % ASTM D 638
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Электрическая прочность, короткое время 22 кВ/мм ASTM D 149
Коэффициент диэлектрических потерь, 1 MГц 0.0003 - ASTM D 150
Относительная электрическая проницаемость, 1 MГц 2.3 - ASTM D 150
Удельное объемное сопротивление 1E16 Ом*см ASTM D 257
Прочие свойстваЗначениеЕдиницаСтандарт
Плотность 920 кг/м³ ASTM D 792
Рекомендации по переработке экструзиейЗначениеЕдиницаСтандарт
Температура расплава 120 - 130 °C -
Особые свойства и характеристики
Способы переработки
Экструзия (прочие виды)
Специальные характеристики
Сшивающийся
Применение
Электрические и электронные устройства
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Латинская Америка
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.