Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® 1248 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® 1248 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Partially bio-circular grade.
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 7 см³/10мин ISO 1133
Температура 300 °C -
Нагрузка 1.2 kg -
Показатель текучести расплава, ПТР 7.5 г/10 мин ISO 1133
Температура 300 °C -
Нагрузка 1.2 kg -
Усадка при литье, продольная 0.8 % ISO 294-4, 2577
Усадка при литье, поперечная 0.8 % ISO 294-4, 2577
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 2250 МПа ISO 527
Напряжение в точке текучести 61 МПа ISO 527
Удлинение в точке текучести 6 % ISO 527
Номинальное удлинение при разрыве >50 % ISO 527
Напряжение при разрыве 70 МПа ISO 527
Удлинение при разрыве 130 % ISO 527
Модуль упругости при изгибе, 23°C 2250 МПа ISO 178
Предел прочности при изгибе 88 МПа ISO 178
Ударная прочность по Шарпи, +23°C N кДж/м2 ISO 179/1eU
Ударная прочность по Шарпи, -30°C N кДж/м2 ISO 179/1eU
Ударная прочность по Шарпи с надрезом, +23°C, 3mm 70 кДж/м2 ISO 179/1eA
Type of failure P - -
Ударная прочность по Шарпи с надрезом, -30°C, 3mm 60 кДж/м2 ISO 179/1eA
Type of failure P(C) - -
Ударная вязкость по Изоду образцов с надрезом, +23°C 65 кДж/м2 ISO 180/1A
Ударная вязкость по Изоду образцов с надрезом 30 кДж/м2 ISO 180/1A
Температура -30 °C -
Прокол - максимальое усилие, +23°C 5200 Н ISO 6603-2
Прокол - максимальое усилие, -30°C 6100 Н ISO 6603-2
Энергия прокола, +23°C 55 Дж ISO 6603-2
Энергия прокола, -30°C 60 Дж ISO 6603-2
Твердость по вдавленному шарику 108 МПа ISO 2039-1
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура стеклования, 10 °C/мин 148 °C ISO 11357-1/-2
Температура изгиба под нагрузкой, 1.80 МПа 125 °C ISO 75-1/-2
Температура изгиба под нагрузкой, 0.45 МПа 139 °C ISO 75-1/-2
Температура размягчения по Вика, B 146 °C ISO 306
Коэффициент линейного теплового расширения, параллельный 70 E-6/K ISO 11359-1/-2
Коэффициент линейного теплового расширения, перпендикулярный 70 E-6/K ISO 11359-1/-2
Поведение при горении образца 1.5 мм ном. толщины HB класс IEC 60695-11-10
Толщина образца 1.5 мм -
Кислородный индекс 30 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 мм -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 мм -
Glow Wire Flammability Index (GWFI) 900 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 мм -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 мм -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 мм -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 мм -
Other Standards[S]
Термопроводность, твердое состояние 0.2 W/(m K) ISO 8302
S: These properties are reported by the producer according standards that are different to our defaults.
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Удельное объемное сопротивление 1E14 Ом*м IEC 62631-3-1
Удельное поверхностное сопротивление 1E16 Ом IEC 62631-3-2
Электрическая прочность 34 кВ/мм IEC 60243-1
Сравнительный показатель пробоя 225 - IEC 60112
Other Standards[S]
Относительная диэлектрическая проницаемость, 100Гц 3.1 - IEC 60250
Относительная диэлектрическая проницаемость, 1МГц 3 - IEC 60250
Коэффициент диэлектрических потерь, 100 Гц 12 E-4 IEC 60250
Коэффициент диэлектрических потерь, 1 MГц 120 E-4 IEC 60250
S: These properties are reported by the producer according standards that are different to our defaults.
Оптические свойстваЗначениеЕдиницаСтандарт
ISO Data
Коэффициент пропускания света 89[1] % ISO 13468-1, -2
Other Standards[S]
Показатель преломления 1.59 - ISO 489
1: 2 mm  S: These properties are reported by the producer according standards that are different to our defaults.
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 0.4 % Sim. to ISO 62
Поглощение влаги 0.12 % Sim. to ISO 62
Плотность 1200 кг/м³ ISO 1183
насыпная плотность 640 кг/м³ -
Параметры изготовления образцов для испытанийЗначениеЕдиницаСтандарт
Данные ISO
Литье под давлением, температура расплава 300 °C ISO 294
Литье под давлением, температура пресс-формы 80 °C ISO 294
Литье под давлением, скорость впрыска 200 мм/с ISO 294
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 120 °C -
Время предварительной сушки 2 - 3 h -
Влажность переработки ≤0.02 % -
Температура расплава 280 - 320 °C -
Температура формы 80 - 120 °C -
Зоны 1 250 - 260 °C -
Зоны 2 270 - 280 °C -
Зоны 3 280 - 290 °C -
Температура сопла 290 - 300 °C -
Обратное давление 5 - 15 МПа -
Особые свойства и характеристики
Способы переработки
Литье под давлением
Особые показатели
Ударопрочный или модифицированный к удару
Сертификаты
Содержит возобновляемые ресурсы, Контакт с пищей, ISCC Plus
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Латинская Америка, Ближний Восток и Африка
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.