Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2620 Powder - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2620 Powder:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Platamid® HX 2620 Powder
Copolyamide Hot Melt Adhesive / Textile Applications


Platamid® HX 2620 Powder is a low melt viscosity copolyamide adhesive powder for the production of fusible interlinings.
Platamid® HX 2620 Powder offers good laundry resistance and good steam resistance at low/medium fusing conditions.


AVAILABLE GRADES
This grade is available in different grain sizes:
- Platamid® HX 2620 PA80 (0-80 µm paste dot)
- Platamid® HX 2620 PRA 170 (0-170 µm double dot)
PACKAGING
- Platamid® HX 2620 PA80 and Platamid® HX 2620 PRA 170 are delivered in 20 kg sealed bags.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Технологические и физические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 41.5 / * см³/10мин ISO 1133
Температура 150 / * °C -
Нагрузка 2.16 / * kg -
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 124 / * °C ISO 11357-1/-3
Особые свойства и характеристики
Вид поставки
Порошок
Специальные характеристики
Сополимер
Доступность материала по регионам
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.