Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Topthane™ 2290E - TPU - Top Polymer Enterprise

Material Data Center offers the following functions for Topthane™ 2290E:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Topthane datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
For more detailed information, please read our brochure
or contact our representatives in your region.
Механические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Модуль при 100% удлинении 9.2 МПа ASTM D 412
Модуль при 300% удлинении 6.8 МПа ASTM D 412
Твердость по Шору А 90 - ASTM D 2240
Стойкость к разрыву 91.8 кН/м ASTM D 624
Предел прочности 32.7 МПа ASTM D 412
Относительное удлинение при разрыве 400 % ASTM D 412
Прочие свойстваЗначениеЕдиницаСтандарт
Плотность 1120 кг/м³ ASTM D 792
Рекомендации по переработке экструзиейЗначениеЕдиницаСтандарт
Type of extrusion profile - -
Температура предварительной сушки 90 - 110 °C -
Время предварительной сушки 3 - 4 h -
Зоны 1 180 - 190 °C -
Зоны 2 190 - 210 °C -
Зоны 3 190 - 210 °C -
Особые свойства и характеристики
Способы переработки
Экструзия труб и шлангов, Экструзия профилированных изделий, Экструзия (прочие виды)
Вид поставки
Гранулы
Химическая стойкость
Общая химическая стойкость, Гидролитически устойчивый, Маслостойкость
Доступность материала по регионам
Страны Азии и Тихого океана
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.