Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® H4320 AT - POM - BASF

Material Data Center offers the following functions for Ultraform® H4320 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
High-molecular-weight grade for the extrusion of semifinished product; particularly thick walled product can be extruded at high output rates; the material also features high thermal stability and low discoloration.

Abbreviated designation according to ISO 1043-1: POM
Designation according to ISO 29988-POM-K,,E-GNR,1-2
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 2.2 см³/10мин ISO 1133
Температура 190 °C -
Нагрузка 2.16 kg -
Усадка при литье, продольная 2.2 % ISO 294-4, 2577
Усадка при литье, поперечная 2.1 % ISO 294-4, 2577
Температура при извлечении из пресс-формы 110 °C -
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 2400 МПа ISO 527
Напряжение в точке текучести 60 МПа ISO 527
Удлинение в точке текучести 11 % ISO 527
Номинальное удлинение при разрыве 31 % ISO 527
Модуль ползучести при растяжении, 1ч 1800 МПа ISO 899-1
Модуль ползучести при растяжении, 1000ч 1300 МПа ISO 899-1
Ударная вязкость по Шарпи, +23°C 280 кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи, -30°C 250 кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи с надрезом, +23°C 6.5 кДж/м2 ISO 179/1eA
Ударная вязкость по Шарпи с надрезом, -30°C 5.5 кДж/м2 ISO 179/1eA
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 163 °C ISO 11357-1/-3
Температура изгиба под нагрузкой, 1.80 МПа 90 °C ISO 75-1/-2
Температура изгиба под нагрузкой, 0.45 МПа 155 °C ISO 75-1/-2
Температура размягчения по Вика, B 150 °C ISO 306
Коэффициент линейного теплового расширения, продольный 120 E-6/K ISO 11359-1/-2
Класс горючести при номинальной толщине 1.5 мм HB класс IEC 60695-11-10
Толщина образца 1.6 мм -
желтая карточка (Yellow Card) да - -
Класс горючести при толщине образца h HB класс IEC 60695-11-10
Толщина образца 0.8 мм -
желтая карточка (Yellow Card) да - -
Кислородный индекс 15 % ISO 4589-1/-2
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Относительная диэлектрическая проницаемость, 100Гц 3.8 - IEC 62631-2-1
Относительная диэлектрическая проницаемость, 1МГц 3.8 - IEC 62631-2-1
Коэффициент диэлектрических потерь, 100 Гц 10 E-4 IEC 62631-2-1
Коэффициент диэлектрических потерь, 1 MГц 50 E-4 IEC 62631-2-1
Удельное объемное сопротивление 1E11 Ом*м IEC 62631-3-1
Удельное поверхностное сопротивление 1E13 Ом IEC 62631-3-2
Электрическая прочность 40 кВ/мм IEC 60243-1
Сравнительный показатель пробоя 600 - IEC 60112
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 1 % Sim. to ISO 62
Поглощение влаги 0.25 % Sim. to ISO 62
Плотность 1400 кг/м³ ISO 1183
Параметры изготовления образцов для испытанийЗначениеЕдиницаСтандарт
Данные ISO
Литье под давлением, температура расплава 200 °C ISO 294
Литье под давлением, температура пресс-формы 90 °C ISO 294
Литье под давлением, скорость впрыска 200 мм/с ISO 294
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 100 °C -
Время предварительной сушки 3 h -
Влажность переработки ≤0.2 % -
Температура расплава 190 - 230 °C -
Температура формы 60 - 120 °C -
Особые свойства и характеристики
Способы переработки
Литье под давлением, Экструзия профилированных изделий, Экструзия листа, Экструзия (прочие виды)
Вид поставки
Гранулы
Добавки
Добавка, улучшающая съем изделия с пресс-формы
Специальные характеристики
Сополимер
Доступность материала по регионам
Другая текстовая информация
Литье под давлением
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
Экструзия других изделий
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 175 - 180 °C
Extrusion, Pipes, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
Экструзия профиля
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Profiles, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
Экструзия листа
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Plates, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.