Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of AVALON® 80 ABX - TPU - Huntsman Polymers Corp.

Material Data Center offers the following functions for AVALON® 80 ABX:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Avalon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
机械性能价值单位Test Standard
Other Standards[S]
拉伸强度 25 MPa DIN 53504
断裂伸长率 650 % DIN 53504
撕裂强度 35 kN/m DIN 53507
耐磨性 55 mm³ DIN 53516
肖氏硬度A 81 - DIN 53505
肖氏硬度D 30 - DIN 53505
S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
Other Standards[S]
密度 1150 kg/m³ DIN 53479
S: These properties are reported by the producer according standards that are different to our defaults.
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 - 90 °C -
预干燥-时间 2 h -
模具温度 25 - 50 °C -
加料温度 25 - 35 °C -
1区 170 - 190 °C -
2区 175 - 195 °C -
3区 175 - 200 °C -
喷嘴温度 170 - 195 °C -
螺杆转速 20 - 80 rpm -
注射压力 2 - 10 MPa -
背压 0.03 - 0.3 MPa -
保压压力 1 - 5 MPa -
典型数据
加工方法
注塑
特征
防滑, 抗划性
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.