Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BMC RF 9/15 - UP-(MD+GF)70 - Polynt S.p.A.

Material Data Center offers the following functions for BMC RF 9/15:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other BMC datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Not resistant. May be used under certain conditions (brief contact).

Please consider the information about the application of the materials.
加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 0.2 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
简支梁冲击强度, +23°C 20 kJ/m² ISO 179/1eU
洛克硬度 M 80 - ISO 2039-2
Other Standards[S]
弯曲模量, 23°C 9000 MPa ISO 14125A
弯曲强度 60 MPa ISO 14125A
S: These properties are reported by the producer according standards that are different to our defaults.
热性能价值单位Test Standard
ISO数据
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 3.0 mm -
Yellow Card 现存 是的 - -
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
电性能价值单位Test Standard
ISO数据
体积电阻率 1E12 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
介电强度 16 kV/mm IEC 60243-1
ASTM数据
耐电弧性 180 s ASTM D 495
其它性能价值单位Test Standard
吸水性 0.2 % 类似ISO 62
密度 1800 kg/m³ ISO 1183
典型数据
加工方法
模压成型
供货形式
块状模材料
特殊性能
阻燃的, 无卤
应用
电子电气
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.