Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BioFibra BF-LHE01 - Polyester-W - FuturaMat

Material Data Center offers the following functions for BioFibra BF-LHE01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Biofibra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
For more detailed information, please read our
or contact our representatives in your region.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 11.2 g/10min ISO 1133
温度 190 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2880 MPa ISO 527
屈服应力 29 MPa ISO 527
屈服伸长率 1.6 % ISO 527
断裂应力 19 MPa ISO 527
弯曲模量, 23°C 3130 MPa ISO 178
简支梁冲击强度, +23°C 15 kJ/m² ISO 179/1eU
肖氏硬度D 79 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 41 °C ISO 75-1/-2
其它性能价值单位Test Standard
密度 1260 kg/m³ ISO 1183
典型数据
加工方法
热成型
Certifications
生物相容, 生物降解
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.