Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bormed™ SB815MO - PP - Borealis A/S

Material Data Center offers the following functions for Bormed™ SB815MO:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bormed datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 1.5 g/10min ISO 1133
温度 230 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 475 MPa ISO 527
屈服应力 17 MPa ISO 527
屈服伸长率 18 % ISO 527
弯曲模量, 23°C 425 MPa ISO 178
简支梁缺口冲击强度, +23°C 80 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 145 °C ISO 11357-1/-3
热变形温度, 0.45 MPa 55 °C ISO 75-1/-2
加工推荐(注塑)价值单位Test Standard
注塑熔体温度 210 - 250 °C -
模具温度 10 - 30 °C -
保压压力 20 - 50 MPa -
加工推荐(挤出)价值单位Test Standard
注塑熔体温度 170 - 190 °C -
1区 170 - 200 °C -
喷嘴温度 180 - 200 °C -
典型数据
加工方法
注塑, 吹塑
特殊性能
透明., 消毒, 蒸汽灭菌
特征
共聚物, 随机共聚物
Certifications
可食品接触的, FDA 21 CFR认证, 医用级, US药物六级认证, Device Master File
应用
药物, 包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.