Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 2061-3 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ 2061-3:
unit conversion, PDF datasheet print, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 3.5 g/10min ISO 1133
温度 300 °C -
负载 1.2 kg -
模塑收缩率, 平行 0.6 % ISO 294-4, 2577
ASTM数据
熔融指数, MFI 3.5 g/10min ASTM D 1238
温度 300 °C -
负载 1.2 kg -
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 2480 MPa ISO 527
屈服应力 60 MPa ISO 527
断裂应力 72.4 MPa ISO 527
断裂伸长率 >50 % ISO 527
弯曲模量, 23°C 2410 MPa ISO 178
Izod冲击强度, +23°C N kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C 93 kJ/m² ISO 180/1A
ASTM数据
拉伸模量 2482 MPa ASTM D 638
屈服应力 60 MPa ASTM D 638
断裂拉伸强度 71.7 MPa ASTM D 638
断裂伸长率 150 % ASTM D 638
弯曲模量 2413 MPa ASTM D 790
弯曲强度 96.5 MPa ASTM D 790
洛克硬度 R 118 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 961 J/m ASTM D 256
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 132 °C ISO 75-1/-2
维卡软化温度, B 151 °C ISO 306
1.5mm名义厚度时的燃烧性 V-2 class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 3.0 mm -
燃烧性-氧指数 26 % ISO 4589-1/-2
ASTM数据
UL94 燃烧性 V-2 - UL 94
测试厚度 0.749 mm -
热释放速率, 平行 68.4 E-6/K ASTM D 696
DTUL @ 264 psi 132 °C ASTM D 648
维卡温度 151 °C ASTM D 1525
其它性能价值单位Test Standard
吸湿性 0.32 % 类似ISO 62
密度 1200 kg/m³ ISO 1183
吸水率, 24小时 0.15 % ASTM D 570
吸水率, 平衡 0.32 % ASTM D 570
密度 1200 kg/m³ ASTM D 792
典型数据
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经热稳处理的/耐热的
耐化学试剂
抗氧化性
应用
药物
地区供应
北美, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.