Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cawiton SN980 - SEBS - Wittenburg B.V.

Material Data Center offers the following functions for Cawiton SN980:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cawiton datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 10.1 g/10min ISO 1133
温度 230 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸强度 6.2 MPa ISO 37
断裂伸长率 431 % ISO 37
70°C时恒定应变下的永久变形, 24h 60 % ISO 815
撕裂强度 39.7 kN/m ISO 34-1
肖氏硬度A 80 - ISO 7619-1
Other Standards[S]
100%应变时的应力 3.9 MPa ISO 37
300%应变时的应力 14.7 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 166 °C ISO 11357-1/-3
其它性能价值单位Test Standard
密度 1170 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
注塑熔体温度 180 - 240 °C -
模具温度 20 - 40 °C -
加料温度 30 - 60 °C -
1区 180 - 220 °C -
2区 190 - 230 °C -
3区 190 - 230 °C -
喷嘴温度 200 - 240 °C -
典型数据
加工方法
注塑, 薄膜挤出成型, 管材挤出, 异型材挤出成型
供货形式
自然色
特殊性能
Opaque
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.