Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELCON® M15HP - POM - Celanese

Material Data Center offers the following functions for CELCON® M15HP:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celcon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 1.3 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
模塑收缩率, 平行 2.3 % ISO 294-4, 2577
模塑收缩率, 垂直 1.9 % ISO 294-4, 2577
熔体密度 1170 kg/m³ -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2800 MPa ISO 527
屈服应力 68 MPa ISO 527
屈服伸长率 16 % ISO 527
无缺口简支梁冲击强度, +23°C 280 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 235 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 11 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 8.5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 173 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 101 °C ISO 75-1/-2
热变形温度, 0.45 MPa 158 °C ISO 75-1/-2
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 120 E-6/K ISO 11359-1/-2
其它性能价值单位Test Standard
吸水性 0.75 % 类似ISO 62
吸湿性 0.2 % 类似ISO 62
密度 1410 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 3 h -
加工湿度 ≤0.35 % -
注塑熔体温度 205 - 220 °C -
模具温度 93 - 121 °C -
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 其它挤出成型, 吹塑, 压延成型
供货形式
粒料
特征
共聚物
Certifications
可水接触的
地区供应
北美, 中南美洲
其他信息
注塑成型
Drying is generally not required because Celcon® and Hostaform® acetal copolymer materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can lead to splay (silver streaking) in molded parts. For better uniformity in molding especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying conditions are 80 c (180 F) for three hours. Desiccant hopper dryers are not required. Max. water content = 0.35%.
Standard reciprocating screw injection molding machines with a high compression screw (minimum 3:1 and preferably 4:1) and low back pressure (0.35 Mpa/50 PSI) are favored. Using a low compression screw (i.e.-general purpose with a 2:1 compression ratio) can result in unmelted particles and poor thermal homogeneity. Using a high back pressure to make up for a low compression ratio may lead to excessive shear heating and deterioration of the Celcon material.

Melt temperature: Preferred range 205-220 C (400-430 F) Melt temperature should never exceed 230 C (450 F).
Mold surface temperature: preferred range 93-121 C (200-250 F) especially with wall thickness less than 1.5 mm (0.060 in.). Wall thickness greater than 3 mm (1/8 in.) may use a cooler (82 C/180 F) mold surface temperature and wall thickness over 6 mm (1/4 in.) may use a cold mold surface temperature as low as 25 C (80 F). In general, mold surface temperatures lower than 82 C (180 F) may produce a hazy surface or a surface with flow lines, pits and other included defects.
Postprocessing conditioning and moisturizing not required. It may be necessary to fixture large or complicated parts with varying wall thickness to prevent warpage while cooling to ambient temperature.
薄膜挤出成型
Drying is generally not required because Celcon materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can cause surface defects on the extruded film. For better uniformity especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying conditions are 3 Hrs. at 80 C (180 F). Desiccant hopper dryers are not required. Max. moisture content = 0.35%.
Standard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high compression ratio of at least 3:1 and preferably 4:1 to assure good melting and melt homogeneity. The design should be approximately 35% each for feed and metering sections with the remaining 30% as the transition zone.

Melt temperature: 160-220 C (320-430 F)
Postprocessing conditioning or moisturizing is not required.
E尾募烦龀尚
Drying is generally not required because Celcon materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can cause surface defects on the extrusion. For better uniformity especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying conditions are 3 Hrs. at 80 C (180 F). Desiccant hopper dryers are not required. Max. moisture content = 0.035%.
Standard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high compression ratio of at least 3:1 and preferably 4:1 to assure good melting and melt homogeneity. The design should be approximately 35% each for feed and metering sections with the remaining 30% as the transition zone.

Melt temperature: 180-220 C (360-430 F).
Postprocessing or moisturizing is not required. For thick walled extrusions (>3 mm or 1/8 in.), annealing is recommended to reduce internal stresses.

Annealing temperature: 130-140 C (265-285 F)
Annealing time: 10 min/mm thickness
吹塑成型
Consult product information services.
Consult product information services.
Consult product information services.
压延成型
Consult product information services.
Consult product information services.
Consult product information services.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.