Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PP-GF50-0403 P10/10 - PP-GLF50 - Celanese

Material Data Center offers the following functions for CELSTRAN® PP-GF50-0403 P10/10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Material code according to ISO 1043-1: PP Heat stabilized polypropylene reinforced with 50 weight percent long glass fibers. Black. The fibers are chemically coupled to the polypropylene matrix. The pellets are cylindrical and normally as well as the embedded fibers 11 mm long. Parts molded of CELSTRAN have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton built in the parts. The long fiber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Application field: Functional/structural parts for automotive

Flammability at thickness h (2 mm)HB-
机械性能价值单位Test Standard
ISO数据
拉伸模量 11600 MPa ISO 527
断裂应力 140 MPa ISO 527
断裂伸长率 1.8 % ISO 527
无缺口简支梁冲击强度, +23°C 60 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 58 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 32 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 33 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 165 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 158 °C ISO 75-1/-2
热变形温度, 8.00 MPa 134 °C ISO 75-1/-2
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 2.0 mm -
其它性能价值单位Test Standard
密度 1340 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 94 °C -
预干燥-时间 2 h -
注塑熔体温度 260 - 290 °C -
模具温度 40 - 70 °C -
函数
应力-应变.  , CELSTRAN® PP-GF50-0403 P10/10, PP-GLF50, Celanese
正割模量-应变.  , CELSTRAN® PP-GF50-0403 P10/10, PP-GLF50, Celanese
典型数据
加工方法
注塑, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 表面涂层, 模压/烧结成型
供货形式
粒料, 黑色
特殊性能
经热稳处理的/耐热的
特征
化学偶合增强, 防蠕变, Long fiber reinforced, 低翘曲
应用
汽车
地区供应
北美, 欧洲, 亚太
其他信息
注塑成型
PP&PE drying requirements: 2 hrs. @94° C.
A dehumidifier or desiccant dryer is recommended.
Celstran can be processed on a standard injection molding unit.
A general purpose metering screw is recommended with a zone
distribution of 40% feed, 40% transition, and 20% metering.
A free flowing check ring assembly is recommended.

Melt Temp: 260-290°C.
Mold Temp: 40- 70°C.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.