Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew EV600-30 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew EV600-30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Cristal™ Renew copolyester EV600-30 is a high flow product designed and engineered specifically for cosmetics

packaging applications. With its unsurpassed color and clarity and an unmatched ability to mold thick parts with

improved gate aesthetics, Cristal Renew EV600-30 is clearly a well-suited copolyester for premium cosmetics

packaging. Other outstanding features of Cristal Renew EV600-30 are excellent chemical resistance, high gloss,

and improvements in processing such as faster cycle times, and lower scrap rates. Cristal Renew EV600-30 is also

ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization

rate, and flow characteristics.

加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.0045 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 1650 MPa ISO 527
屈服应力 47 MPa ISO 527
屈服伸长率 4.2 % ISO 527
断裂应力 28.9 MPa ISO 527
断裂伸长率 195 % ISO 527
ASTM数据
拉伸模量 1813 MPa ASTM D 638
屈服应力 47.4 MPa ASTM D 638
断裂拉伸强度 51.9 MPa ASTM D 638
屈服伸长率 4 % ASTM D 638
断裂伸长率 322 % ASTM D 638
弯曲模量 1927 MPa ASTM D 790
洛克硬度 R 102,3 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 934 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 65.7 J/m ASTM D 256
温度 -40 °C -
Izod冲击强度, 1/8 in 2460 J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 71.5 °C ASTM D 648
DTUL @ 264 psi 63.5 °C ASTM D 648
光学特性价值单位Test Standard
ASTM数据
雾度 0.3 % ASTM D 1003
光透射率 91.9 % ASTM D 1003
其它性能价值单位Test Standard
密度 1250 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 65 °C -
预干燥-时间 8 h -
注塑熔体温度 218 - 240 °C -
模具温度 16 - 38 °C -
典型数据
加工方法
注塑, 其它挤出成型
特殊性能
高冲击韧性的/经抗冲改性的, 透明.
特征
High Gloss, 共聚物
耐化学试剂
通用耐化学性
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.