Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CYCOLOY™ FR Resin CX7240 - Europe - (PC+ABS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for CYCOLOY™ FR Resin CX7240 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Cycoloy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
CYCOLOY CX7240 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, medium flow, non chlorinated/brominated flame retardant grade. It has a UL94 V0@.75mm, 5VA@3.0mm and 5VB@1.5mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications.

UL Yellow Card Link E45329-549531
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 15 cm³/10min ISO 1133
温度 260 °C -
载荷 2.16 kg -
熔体密度 1060 kg/m³ -
熔体 0.24 W/(m K) -
熔体的比热 2050 J/(kg K) -
喷射温度 94 °C -
ASTM数据
熔融指数, MFI 18 g/10min ASTM D 1238
温度 260 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2600 MPa ISO 527
屈服应力 65 MPa ISO 527
屈服伸长率 4 % ISO 527
断裂应力 50 MPa ISO 527
断裂伸长率 50 % ISO 527
弯曲模量 2500 MPa ISO 178
简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 22 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 10 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C, 4mm 25 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, -30°C, 4mm 10 kJ/m² ISO 180/1A
ASTM数据
拉伸模量 2600 MPa ASTM D 638
屈服应力 65 MPa ASTM D 638
断裂拉伸强度 58 MPa ASTM D 638
屈服伸长率 4.1 % ASTM D 638
断裂伸长率 100 % ASTM D 638
弯曲模量 2500 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 700 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 175 J/m ASTM D 256
温度 -30 °C -
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 93 °C ISO 75-1/-2
维卡软化温度, B 110 °C ISO 306
维卡软化温度, 120°C/h 50N 113 °C ISO 306
线性热膨胀系数, 平行 77 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 77 E-6/K ISO 11359-1/-2
厚度为h时的燃烧性 V-2 class IEC 60695-11-10
测试用试样的厚度 0.4 mm -
厚度为h时的5V燃烧性 5VB class IEC 60695-11-20
测试用试样的厚度 1.5 mm -
热导率 0.2 W/(m K) DIN 52616
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝引燃温度 (GWIT) 800 °C IEC 60695-2-13
GWIT - 测试用试样厚度 2 mm -
灼热丝引燃温度 (GWIT) 800 °C IEC 60695-2-13
GWIT - 测试用试样厚度 3 mm -
ASTM数据
DTUL @ 66 psi 100 °C ASTM D 648
DTUL @ 264 psi 89 °C ASTM D 648
维卡温度 110 °C ASTM D 1525
电性能价值单位Test Standard
ISO数据
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 35 kV/mm IEC 60243-1
其它性能价值单位Test Standard
吸水性 0.2 % 类似ISO 62
吸湿性 0.1 % 类似ISO 62
密度 1200 kg/m³ ISO 1183
密度 1190 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 - 90 °C -
预干燥-时间 2 - 4 h -
加工湿度 ≤0.02 % -
注塑熔体温度 250 - 300 °C -
模具温度 60 - 85 °C -
加料温度 60 - 80 °C -
1区 230 - 280 °C -
2区 240 - 290 °C -
3区 250 - 300 °C -
函数
粘度-剪切速度 , CYCOLOY™ FR Resin CX7240 - Europe, (PC+ABS), SABIC
剪切应力-剪切速度 , CYCOLOY™ FR Resin CX7240 - Europe, (PC+ABS), SABIC
比容-温度(pvT) , CYCOLOY™ FR Resin CX7240 - Europe, (PC+ABS), SABIC
典型数据
加工方法
注塑
添加剂
阻燃剂
特殊性能
阻燃的
耐化学试剂
通用耐化学性
应用
汽车
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.