Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Dynaflex™ G2706-1000-00 - TPE - Avient Corporation

Material Data Center offers the following functions for Dynaflex™ G2706-1000-00:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dynaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 1 g/10min ASTM D 1238
温度 200 °C -
负载 5 kg -
模压收缩率, 平行 0.05 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
100%伸长率时的模量 0.621 MPa ASTM D 412
300%伸长率时的模量 0.63 MPa ASTM D 412
邵氏硬度A 28 - ASTM D 2240
撕裂强度 14 kN/m ASTM D 624
压缩形变, 22小时 @ 73 °F 8 % ASTM D 395
断裂拉伸强度 5.52 MPa ASTM D 412
断裂伸长率 660 % ASTM D 412
其它性能价值单位Test Standard
密度 890 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
模具温度 15.6 - 37.8 °C -
1区 160 - 199 °C -
2区 171 - 210 °C -
3区 188 - 227 °C -
喷嘴温度 188 - 227 °C -
螺杆转速 25 - 75 rpm -
注射速度 25.4 - 127 mm/s -
背压 0 - 0.758 MPa -
保压压力 0.931 - 2.07 MPa -
典型数据
加工方法
注塑, 其它挤出成型
供货形式
粒料
特殊性能
透明.
特征
好粘附性能, 软质
Certifications
可食品接触的, 10/2011认证, FDA 21 CFR认证, US药物六级认证
应用
汽车, 药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.