Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ CN015-25 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ CN015-25:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastar™ Renew CN015-25 Natural copolyester is a high flow product that contains a mold release to provide ease of demolding. Designed specifically for the unique requirements of luxury cosmetic packaging, our premier PCTA copolyester delivers unsurpassed color and clarity and a capability to mold thick parts with improved gate

aesthetics. Other outstanding features of Eastar™ Renew CN015-25 Natural copolyester include excellent chemical resistance, high gloss, and process enhancements such as faster drying times, faster cycle times, and lower scrap

rates. Eastar™ Renew CN015-25 Natural copolyester is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.003 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
屈服应力 50 MPa ASTM D 638
断裂拉伸强度 35 MPa ASTM D 638
屈服伸长率 4.5 % ASTM D 638
断裂伸长率 193 % ASTM D 638
弯曲模量 1800 MPa ASTM D 790
弯曲强度 67 MPa ASTM D 790
洛克硬度 R 105 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 70 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 38 J/m ASTM D 256
温度 -40 °C -
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 71 °C ASTM D 648
DTUL @ 264 psi 63 °C ASTM D 648
光学特性价值单位Test Standard
ASTM数据
雾度 0.6 % ASTM D 1003
光透射率 90 % ASTM D 1003
其它性能价值单位Test Standard
密度 1200 kg/m³ ASTM D 792
加工推荐(挤出)价值单位Test Standard
预干燥-温度 60 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 225 - 245 °C -
模具温度 16 - 50 °C -
典型数据
加工方法
其它挤出成型
供货形式
自然色
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 透明.
特征
可热封的, High Gloss, 共聚物
耐化学试剂
通用耐化学性
Certifications
ISCC Plus
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com