Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ MB002 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ MB002:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastar™ copolyester MB002 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and EtO sterilization. It is a resin specifically developed for extrusion blow molding containers in medical applications where aesthetics such as high clarity and gloss, coupled with high toughness and chemical resistance, are desirable. Compared to many commonly used materials, Eastar™ copolyester MB002 runs on most standard processing equipment with broader processing conditions, and its toughness and melt strength enable

blow molding of larger containers with greater design flexibility. This product meets the biocompatibility requirements under FDA/ISO 10993 and USP Class 6, Plastics.




加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.003 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
拉伸模量 1900 MPa ASTM D 638
屈服应力 47 MPa ASTM D 638
断裂拉伸强度 48 MPa ASTM D 638
屈服伸长率 5 % ASTM D 638
断裂伸长率 300 % ASTM D 638
弯曲模量 1900 MPa ASTM D 790
弯曲强度 65 MPa ASTM D 790
洛克硬度 R 105 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in N J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 63 J/m ASTM D 256
温度 -40 °C -
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 73 °C ASTM D 648
DTUL @ 264 psi 63 °C ASTM D 648
维卡温度 85 °C ASTM D 1525
光学特性价值单位Test Standard
ASTM数据
光泽度 143 - ASTM D 2457
雾度 1.3 % ASTM D 1003
光透射率 91 % ASTM D 1003
其它性能价值单位Test Standard
密度 1250 kg/m³ ASTM D 792
典型数据
加工方法
吹塑
特殊性能
透明., 消毒, 环氧乙烷灭菌(EtO), Gamma irradiation sterilization
特征
颜色稳定性, High Gloss, 熔体强度, 共聚物
耐化学试剂
通用耐化学性, 耐溶剂性, 抗辐射性
Certifications
可食品接触的, FDA 21 CFR认证, 医用级, Biocompatibility ISO 10993, US药物六级认证
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.