Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ecovio® F2223 - (PBAT+PLA) - BASF

Material Data Center offers the following functions for ecovio® F2223:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecovio datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 5.5 cm³/10min ISO 1133
温度 190 °C -
载荷 5 kg -
光学特性价值单位Test Standard
ASTM数据
光透射率 85 % ASTM D 1003
其它性能价值单位Test Standard
密度 1250 kg/m³ ISO 1183
Bulk density 720 kg/m³ -
机械性能(薄膜)价值单位Test Standard
ISO数据
拉伸模量, 平行 760 MPa ISO 527-3
拉伸模量, 垂直 350 MPa ISO 527-3
最大应力, 平行 47 MPa ISO 527-3
最大应力, 平行 43 MPa ISO 527-3
最大应变, 平行 450 % ISO 527-3
最大应变, normal 600 % ISO 527-3
埃尔曼多夫撕裂强度, 平行 0.5 N ISO 6383-2
埃尔曼多夫撕裂强度, 垂直 0.45 N ISO 6383-2
挤出形式 麓碌陇 - -
试样厚度 0.03 mm -
典型数据
加工方法
吹塑挤出成型
供货形式
粒料
特征
共混树脂, 少气味, 熔体强度, 热稳定性, 可焊的
Certifications
生物相容, 生物降解, 可食品接触的, 可堆肥 ISO 13432 (制造商), 可堆肥 ASTM D6400 (制造商), 可堆肥 ISO 13432 (证书), 可堆肥 ASTM D6400 (证书)
应用
包装
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.