Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1154 D FHF - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1154 D FHF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
DESCRIPTION
Elastollan 1154 D FHF is a halogen free, flame retarded polyether based TPU

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at low temperature,
resistance to microbiological attack, good wear performance,
high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing, hoses, profiles

OTHER HINTS
predrying: 2-3h at 100-110°C,
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
机械性能价值单位Test Standard
ISO数据
拉伸模量 160 MPa ISO 527
简支梁缺口冲击强度, +23°C 50 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 3 kJ/m² ISO 179/1eA
100%应变时的应力 19 MPa ISO 527
300%应变时的应力 33 MPa ISO 527
断裂应力 TPE 30 MPa ISO 527
断裂应变 TPE >300 % ISO 527
23°C时恒定应变下的永久变形, 24h 30 % ISO 815
70°C时恒定应变下的永久变形, 24h 45 % ISO 815
撕裂强度 110 kN/m ISO 34-1
耐磨性 40 mm³ ISO 4649
肖氏硬度D 55 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 3.0 mm -
Yellow Card 现存 是的 - -
其它性能价值单位Test Standard
密度 1270 kg/m³ ISO 1183
函数
粘度-剪切速度 , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
剪切应力-剪切速度 , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
动态剪切模量-温度 , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
应力-应变(TPE) , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
典型数据
加工方法
注塑, 异型材挤出成型
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com