Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1180 A - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1180 A:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
DESCRIPTION
Elastollan 1180 A is a polyether based TPU

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at low temperature,
resistance to microbiological attack, good wear performance,
high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing, plugs and terminations, hoses, damping elements,
profiles

OTHER HINTS
predrying: 2-3h at 100-110°C (air circulating oven)
or 80-90°C (dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
机械性能价值单位Test Standard
ISO数据
拉伸模量 15 MPa ISO 527
50%伸长率时的应力S 3 MPa ISO 527
断裂伸长率 >50 % ISO 527
简支梁缺口冲击强度, +23°C N kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C N kJ/m² ISO 179/1eA
拉伸缺口冲击强度, +23°C 500 kJ/m² ISO 8256/1
300%应变时的应力 8 MPa ISO 527
断裂应力 TPE 45 MPa ISO 527
断裂应变 TPE >300 % ISO 527
23°C时恒定应变下的永久变形, 24h 25 % ISO 815
70°C时恒定应变下的永久变形, 24h 45 % ISO 815
撕裂强度 55 kN/m ISO 34-1
耐磨性 30 mm³ ISO 4649
肖氏硬度A 80 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min -44 °C ISO 11357-1/-2
厚度为h时的燃烧性 HB class IEC 60695-11-10
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
介质损耗因子, 100Hz 360 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 1120 E-4 IEC 62631-2-1
体积电阻率 1E9 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
介电强度 39 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 2 % 类似ISO 62
密度 1110 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 200 °C ISO 294
注塑, 模具温度 60 °C ISO 294
函数
粘度-剪切速度 , Elastollan® 1180 A, (TPU-ARET), BASF PU
剪切应力-剪切速度 , Elastollan® 1180 A, (TPU-ARET), BASF PU
动态剪切模量-温度 , Elastollan® 1180 A, (TPU-ARET), BASF PU
应力-应变.  , Elastollan® 1180 A, (TPU-ARET), BASF PU
正割模量-应变.  , Elastollan® 1180 A, (TPU-ARET), BASF PU
应力-应变(TPE) , Elastollan® 1180 A, (TPU-ARET), BASF PU
典型数据
加工方法
注塑, 异型材挤出成型
供货形式
粒料
地区供应
其他信息
注塑成型
Barrel temperature : 195 - 205 °C
Melt temperature : 205 °C
Mold temperature: 25 - 40 °C
E尾募烦龀尚
Barrel temperature : 160 - 180 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.