Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® C 64 D - (TPU-ARES) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® C 64 D:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
DESCRIPTION
Elastollan C 64 D is a polyester based TPU

SPECIAL PROPERTIES
high tensile strength, excellent tear strength,
very good damping behavior, good rebound elasticity,
very good wear performance, good flexibility at low temperature
and resistance to hydrolysis

TYPICAL APPLICATIONS
technical parts, bushes

OTHER HINTS
predrying: 2-3h at 100-110°C
(air circulating oven or dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
机械性能价值单位Test Standard
ISO数据
拉伸模量 390 MPa ISO 527
50%伸长率时的应力S 18 MPa ISO 527
断裂伸长率 >50 % ISO 527
简支梁缺口冲击强度, +23°C N kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 9 kJ/m² ISO 179/1eA
拉伸缺口冲击强度, +23°C 390 kJ/m² ISO 8256/1
100%应变时的应力 24 MPa ISO 527
300%应变时的应力 35 MPa ISO 527
断裂应力 TPE 45 MPa ISO 527
断裂应变 TPE >300 % ISO 527
23°C时恒定应变下的永久变形, 24h 40 % ISO 815
70°C时恒定应变下的永久变形, 24h 55 % ISO 815
撕裂强度 200 kN/m ISO 34-1
耐磨性 25 mm³ ISO 4649
肖氏硬度D 61 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min -14 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 49 °C ISO 75-1/-2
热变形温度, 0.45 MPa 101 °C ISO 75-1/-2
电性能价值单位Test Standard
ISO数据
介质损耗因子, 100Hz 440 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 510 E-4 IEC 62631-2-1
体积电阻率 1E13 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 31 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
密度 1240 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 236 °C ISO 294
注塑, 模具温度 60 °C ISO 294
函数
动态剪切模量-温度 , Elastollan® C 64 D, (TPU-ARES), BASF PU
应力-应变.  , Elastollan® C 64 D, (TPU-ARES), BASF PU
正割模量-应变.  , Elastollan® C 64 D, (TPU-ARES), BASF PU
应力-应变(TPE) , Elastollan® C 64 D, (TPU-ARES), BASF PU
应力-应变(等时的) 23°C, Elastollan® C 64 D, (TPU-ARES), BASF PU
蠕变模量-时间. 23°C, Elastollan® C 64 D, (TPU-ARES), BASF PU
蠕变曲线 23°C, Elastollan® C 64 D, (TPU-ARES), BASF PU
典型数据
加工方法
注塑
供货形式
粒料
地区供应
其他信息
注塑成型
Barrel temperature : 210 - 225 °C
Melt temperature : 225 °C
Mold temperature: 25 - 60 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.