Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Elastron V - TPV - Elastron Kimya A.S

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Elastron V" in Material Data Center leads to the following information:

Tradename: Elastron V
Family: TPV
Producer: Elastron Kimya A.S
86 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Elastron V100.A50.B TPV
Elastron V100.A50.N TPV
Elastron V100.A55.B TPV
Elastron V100.A55.N TPV
Elastron V100.A60.B TPV
Elastron V100.A60.N TPV
Elastron V100.A65.B TPV
Elastron V100.A65.N TPV
Elastron V100.A73.B TPV
Elastron V100.A73.N TPV
Elastron V100.A78.B TPV
Elastron V100.A78.N TPV
Elastron V100.A85.B TPV
Elastron V100.A85.N TPV
Elastron V100.D40.B TPV
Elastron V100.D40.N TPV
Elastron V101.A35.B TPV
Elastron V101.A35.N TPV
Elastron V101.A47.B TPV
Elastron V101.A47.N TPV
Elastron V101.A50.B TPV
Elastron V101.A50.N TPV
Elastron V101.A55.B TPV
Elastron V101.A55.N TPV
Elastron V101.A60.B TPV
Elastron V101.A60.N TPV
Elastron V101.A65.B TPV
Elastron V101.A65.N TPV
Elastron V101.A72.B TPV
Elastron V101.A72.N TPV
Elastron V101.A79.B TPV
Elastron V101.A79.N TPV
Elastron V101.A86.B TPV
Elastron V101.A86.N TPV
Elastron V101.A90.B TPV
Elastron V101.A90.N TPV
Elastron V101.D35.B TPV
Elastron V101.D35.B.U TPV
Elastron V101.D35.N TPV
Elastron V101.D40.B TPV
Elastron V101.D40.N TPV
Elastron V101.D51.B TPV
Elastron V101.D51.N TPV
Elastron V201.A40.B TPV
Elastron V201.A40.N TPV
Elastron V201.A56.B TPV
Elastron V201.A56.N TPV
Elastron V201.A65.B TPV
Elastron V201.A65.N TPV
Elastron V201.A68.B TPV
Elastron V201.A68.N TPV
Elastron V201.A73.B TPV
Elastron V201.A73.N TPV
Elastron V201.A78.B TPV
Elastron V201.A78.N TPV
Elastron V201.A87.B TPV
Elastron V201.A87.N TPV
Elastron V201.A90.B TPV
Elastron V201.A90.N TPV
Elastron V201.D40.B TPV
Elastron V201.D40.N TPV
Elastron V201.D51.B TPV
Elastron V201.D51.N TPV
Elastron V250.A58.B TPV
Elastron V250.A65.B TPV
Elastron V250.A75.B TPV
Elastron V251.A65.B TPV
Elastron V251.A65.N TPV
Elastron V251.A77.B TPV
Elastron V601.A60.B TPV
Elastron V601.A60.N TPV
Elastron V601.A65.N TPV
Elastron V601.A70.B TPV
Elastron V601.A70.N TPV
Elastron V601.A75.B TPV
Elastron V601.A75.N TPV
Elastron V601.A80.B TPV
Elastron V601.A80.N TPV
Elastron V601.A85.B TPV
Elastron V601.A85.N TPV
Elastron V601.A90.B TPV
Elastron V601.A90.N TPV
Elastron V601.A93.B TPV
Elastron V601.A93.N TPV
Elastron V601.A95.B TPV
Elastron V601.A95.N TPV

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.