Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of G-PAEK™ 1230GF - PEK-GF30 - Gharda Plastics Limited

Material Data Center offers the following functions for G-PAEK™ 1230GF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other G-PAEK datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.003 mm/mm ASTM D 955
模压收缩率, TD 0.01 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
拉伸模量 11500 MPa ASTM D 638
拉伸强度 185 MPa ASTM D 638
断裂伸长率 2.5 % ASTM D 638
弯曲模量 10500 MPa ASTM D 790
弯曲强度 280 MPa ASTM D 790
洛克硬度 M 105 - ASTM D 785
邵氏硬度D 90 - ASTM D 2240
悬臂梁缺口冲击强度, 1/8 in 60 J/m ASTM D 256
Izod冲击强度, 1/8 in 610 J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
UL94 燃烧性 V-0 - UL 94
测试厚度 0.8 mm -
DTUL @ 264 psi 360 °C ASTM D 648
熔点 372 °C ASTM D 3418
玻璃化转变温度 152 °C ASTM E 1356
电性能价值单位Test Standard
ASTM数据
电介质强度, 短时 14 kV/mm ASTM D 149
表面电阻率 >1E15 Ohm ASTM D 257
体积电阻率 >1E15 Ohm*cm ASTM D 257
耐电弧性 160 s ASTM D 495
其它性能价值单位Test Standard
密度 1500 kg/m³ ASTM D 792
典型数据
加工方法
注塑
供货形式
碎粒料
特殊性能
阻燃的, 经热稳处理的/耐热的
耐化学试剂
通用耐化学性
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.