Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of GREENFLEX® ML 30 - EVAC - Versalis S.p.A

Material Data Center offers the following functions for GREENFLEX® ML 30:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Greenflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection moulding and extrusion,
Parts produced with Greenflex ML 30 show good elasticity performances and good ESCR resistance.  

Applications
Gaskets, especially when food contact is required, profiles and flexible items.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 2.5 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
熔体密度 787 kg/m³ -
熔体 0.2 W/(m K) -
熔体的比热 2540 J/(kg K) -
喷射温度 74 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 90 MPa ISO 527
肖氏硬度A 94 - ISO 7619-1
肖氏硬度D 42 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 97 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 85 °C ISO 11357-1/-2
线性热膨胀系数, 平行 125 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 75 kV/mm IEC 60243-1
其它性能价值单位Test Standard
密度 929 kg/m³ ISO 1183
函数
粘度-剪切速度 , GREENFLEX®  ML 30, EVAC, Versalis
剪切应力-剪切速度 , GREENFLEX®  ML 30, EVAC, Versalis
典型数据
加工方法
注塑
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型

#2

Typical processing temperature range:

    Melt temperature         150 - 210 °C

    Mold temperature          10 -  30  °C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.