Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of INNOPRENE 1640 N - TPE - Kumho Polychem

Material Data Center offers the following functions for INNOPRENE 1640 N:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Innoprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
机械性能价值单位Test Standard
ISO数据
拉伸强度 6.9 MPa ISO 37
70°C时恒定应变下的永久变形, 24h 35 % ISO 815
撕裂强度 34.3 kN/m ISO 34-1
肖氏硬度A 65 - ISO 7619-1
ASTM数据
100%伸长率时的模量 2.4 MPa ASTM D 412
邵氏硬度A 65 - ASTM D 2240
撕裂强度 34.3 kN/m ASTM D 624
压缩形变, 22 hr @ 158 °F 35 % ASTM D 395
拉伸强度 6.9 MPa ASTM D 412
其它性能价值单位Test Standard
密度 950 kg/m³ ISO 1183
密度 950 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 85 °C -
预干燥-时间 3 h -
注塑熔体温度 190 - 230 °C -
模具温度 10 - 60 °C -
1区 160 - 180 °C -
2区 180 - 200 °C -
3区 200 °C -
喷嘴温度 200 - 220 °C -
加工推荐(挤出)价值单位Test Standard
预干燥-温度 85 °C -
预干燥-时间 3 h -
注塑熔体温度 190 - 230 °C -
加料温度 160 - 170 °C -
1区 180 - 200 °C -
2区 180 - 200 °C -
3区 180 - 200 °C -
喷嘴温度 180 - 210 °C -
典型数据
加工方法
注塑, 管材挤出, 异型材挤出成型, 片材挤出成型, 电线挤出, 吹塑, 压延成型
供货形式
粒料, 自然色
特殊性能
经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
特征
防老
耐化学试剂
通用耐化学性, 抗臭氧性
应用
通用
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.