Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of K-Resin® KR03E - SB - INEOS Styrolution

Material Data Center offers the following functions for K-Resin® KR03E:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other K-Resin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
K-Resin® KR03E processes very well in injection molding, providing good cycle times and design flexibility. K-Resin® KR03E alone or in blends, can be extruded into sheet and thermoformed on conventional equipment at high output rates. The favorable economics of K-Resin® SBC, along with high productivity, have made possible tough clear disposable drinking cups, lids and other packaging applications. K-Resin® KR03E will process on most conventional equipment, allowing the molder to run a crystal clear bottle without expensive machine modifications, special molds, different screws, or dryers. K-Resin® KR03 can be blow molded in a broad range of sizes and shapes, from small pill bottles and medical drainage units, to very tall display bottles. It also can be injection blow molded into extremely high impact bottles with glass-like clarity.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 7.5 cm³/10min ISO 1133
温度 200 °C -
载荷 5 kg -
熔融指数, MFI 7.5 g/10min ISO 1133
温度 200 °C -
负载 5 kg -
模塑收缩率, 平行 0.7 % ISO 294-4, 2577
熔体密度 907 kg/m³ -
熔体 0.184 W/(m K) -
熔体的比热 2300 J/(kg K) -
喷射温度 60 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 1500 MPa ISO 527
屈服应力 25 MPa ISO 527
屈服伸长率 2.2 % ISO 527
名义断裂伸长率 >50 % ISO 527
弯曲模量, 23°C 1400 MPa ISO 178
弯曲强度 30 MPa ISO 178
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 2 kJ/m² ISO 179/1eA
肖氏硬度D 63 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 61 °C ISO 75-1/-2
热变形温度, 0.45 MPa 76 °C ISO 75-1/-2
维卡软化温度, A 88 °C ISO 306
维卡软化温度, B 60 °C ISO 306
光学特性价值单位Test Standard
ASTM数据
雾度 1.5 % ASTM D 1003
光透射率 91 % ASTM D 1003
其它性能价值单位Test Standard
吸湿性 0.07 % 类似ISO 62
密度 1010 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 50 °C -
预干燥-时间 3 - 4 h -
注塑熔体温度 180 - 240 °C -
模具温度 30 - 50 °C -
典型数据
加工方法
注塑, 片材挤出成型, 吹塑, 热成型
供货形式
粒料
特殊性能
高冲击韧性的/经抗冲改性的, 透明.
特征
共混树脂, High Gloss, 共聚物
Certifications
可食品接触的
应用
IT/商务机器, 药物, 包装, 玩具
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
As a rule, the K-Resin® granules do not have to be pre-dried. However, in the event of unfavorable storage or transportation conditions involving severe temperature fluctuations, moisture can condense on the surface of the granules and this then has to be removed in a pre-drying step. The granules should be pre-dried in a dry-air dryer for 3 to 4 hours at a temperature of about 50°C.

PROCESSING

Melt temperature, range: 180 - 240°C

Mold temperature, range: 30 - 50°C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.