Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KPX1067 - PP-(GF+MF) - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KPX1067:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.004 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸强度 75 MPa ISO 527
弯曲模量 4500 MPa ISO 178
弯曲强度 105 MPa ISO 178
简支梁冲击强度, +23°C 45 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 7 kJ/m² ISO 179/1eA
洛克硬度 R 110 - ISO 2039-2
ASTM数据
拉伸模量 5300 MPa ASTM D 638
拉伸强度 70 MPa ASTM D 638
弯曲模量 4600 MPa ASTM D 790
弯曲强度 110 MPa ASTM D 790
洛克硬度 R 105 - ASTM D 785
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 163 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 150 °C ISO 75-1/-2
热变形温度, 0.45 MPa 150 °C ISO 75-1/-2
厚度为h时的燃烧性 HB class IEC 60695-11-10
ASTM数据
UL94 燃烧性 HB - UL 94
DTUL @ 66 psi 150 °C ASTM D 648
DTUL @ 264 psi 147 °C ASTM D 648
熔点 163 °C ASTM D 3418
其它性能价值单位Test Standard
密度 1220 kg/m³ ISO 1183
密度 1240 kg/m³ ASTM D 792
典型数据
应用
汽车
地区供应
北美, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.