Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar® Film 302 PGM TR - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar® Film 302 PGM TR:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Kynar® film 302 PGM TR is a flexible thermoplastic fluorinated film. The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior. These films are specially designed for photovoltaic applications.
电性能价值单位Test Standard
ISO数据
介电强度 110 kV/mm IEC 60243-1
其它性能价值单位Test Standard
吸湿性 0.2 % 类似ISO 62
密度 1400 kg/m³ ISO 1183
机械性能(薄膜)价值单位Test Standard
ISO数据
屈服应力, 平行 45 MPa ISO 527-3
屈服应力, 垂直 45 MPa ISO 527-3
屈服应变., 平行 11 % ISO 527-3
屈服应变., 垂直 11 % ISO 527-3
最大应力, 平行 30 MPa ISO 527-3
最大应力, 垂直 30 MPa ISO 527-3
最大应变, 平行 100 % ISO 527-3
最大应变, 垂直 50 % ISO 527-3
继续撕裂强度, 平行 2 N/mm ISO 6383-1
继续撕裂强度, 垂直 3 N/mm ISO 6383-1
挤出形式 麓碌陇 - -
试样厚度 0.03 mm -
典型数据
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.