Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LIM® 6040 - VMQ - Momentive Performance Materials Inc.

Material Data Center offers the following functions for LIM® 6040:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other LIM datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Appearance/Color:
liquid, transparent

Characteristics:
fast cure, high tear strength

Conformity:
The product meets the requirements for passing the test standards USP Class VI, FDA 21 CFR 177.2600 and ISO 10993.
Based on listing of ingredients in the BfR recommendation XV "Silicones", the product is compositionally compliant.

These values were determined with the following conditions:
Postbaked 1 hr @ 204ºC / 400ºF.

Other values were achieved with the following conditions:
As Molded 30 sec @ 177ºC / 350ºF:


Property Value Unit Standard
Shore A hardness, 3s 40 - ISO 868
Tensile Strength 8.3 MPa
ISO 37
Strain at break 650 %
ISO 37
Tear Strength 40,4 kN/m
ASTM D 624
机械性能价值单位Test Standard
ISO数据
拉伸强度 9 MPa ISO 37
断裂伸长率 600 % ISO 37
肖氏硬度A 42 - ISO 7619-1
ASTM数据
撕裂强度 39 kN/m ASTM D 624
热性能价值单位Test Standard
ISO数据
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
Yellow Card 现存 是的 - -
其它性能价值单位Test Standard
密度 1120 kg/m³ ISO 1183
典型数据
加工方法
注塑
特殊性能
透明.
Certifications
可食品接触的, 食品接触批准 BfR, FDA 21 CFR认证, US药物六级认证
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.