Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LIGHTER™ S93 - PET - Equipolymers Global

Material Data Center offers the following functions for LIGHTER™ S93:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lighter datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
机械性能价值单位Test Standard
ISO数据
拉伸模量 2300 MPa ISO 527
屈服应力 55 MPa ISO 527
屈服伸长率 4 % ISO 527
断裂应力 24 MPa ISO 527
断裂伸长率 250 % ISO 527
弯曲模量, 23°C 2100 MPa ISO 178
悬臂梁缺口冲击强度, +23°C 4.5 kJ/m² ISO 180/1A
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 247 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 78 °C ISO 11357-1/-2
维卡软化温度, B 77 °C ISO 306
线性热膨胀系数, 平行 83 E-6/K ISO 11359-1/-2
其它性能价值单位Test Standard
Intrinsic Viscosity 0.8 dl/g -
乙醛 1 ppm -
Color b 1.5 - CIE
Crystallinity 50 % -
Moisture Content 0.4 % -
Bulk density 880 kg/m³ -
加工推荐(注塑)价值单位Test Standard
注塑熔体温度 277 °C -
模具温度 20 °C -
典型数据
加工方法
注塑, 吹塑
特征
共聚物
Certifications
可食品接触的
应用
包装
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.