Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Lucalen A 2700M - (PE-LD) - LyondellBasell Industries

Material Data Center offers the following functions for Lucalen A 2700M:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lucalen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 7.2 g/10min ISO 1133
温度 190 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
断裂应力 11 MPa ISO 527
断裂伸长率 >50 % ISO 527
弯曲模量, 23°C 42 MPa ISO 178
悬臂梁缺口冲击强度 N kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -40 °C -
肖氏硬度D 30 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 95 °C ISO 11357-1/-3
维卡软化温度, A 60 °C ISO 306
其它性能价值单位Test Standard
密度 924 kg/m³ ISO 1183
典型数据
加工方法
注塑, 吹塑挤出成型, 薄膜挤出成型, 管材挤出, 片材挤出成型, 电线挤出, 其它挤出成型, 模压成型
供货形式
粒料, 自然色
特殊性能
高冲击韧性的/经抗冲改性的
特征
好粘附性能, 软质, 可焊的
耐化学试剂
通用耐化学性, 耐环境应力裂纹性
Certifications
可食品接触的, 1935/2004/EC认证, 10/2011认证
地区供应
欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.