Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUMICENE® mPE M 2735 - PE - TotalEnergies

Material Data Center offers the following functions for LUMICENE® mPE M 2735:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lumicene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 3.5 g/10min ISO 1133
温度 190 °C -
负载 2.16 kg -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 119 °C ISO 11357-1/-3
光学特性价值单位Test Standard
ISO Data
浑浊率 1.3 - ISO 14782
ASTM数据
光泽度 89 - ASTM D 2457
其它性能价值单位Test Standard
密度 927 kg/m³ ISO 1183
机械性能(薄膜)价值单位Test Standard
ISO数据
屈服应力, 平行 9 MPa ISO 527-3
屈服应力, normal 9 MPa ISO 527-3
断裂应力, 平行 39 MPa ISO 527-3
断裂应力, 垂直 24 MPa ISO 527-3
最大应变, 平行 470 % ISO 527-3
最大应变, normal 530 % ISO 527-3
落镖试验A 100 g ISO 7765-1
挤出形式 陆陇 - -
试样厚度 0.2 mm -
加工推荐(挤出)价值单位Test Standard
注塑熔体温度 240 - 280 °C -
典型数据
加工方法
薄膜挤出成型
特殊性能
高冲击韧性的/经抗冲改性的
特征
Good Drawdown, 低边缘收缩性
耐化学试剂
抗氧化性
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.