Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY PC 1201-22 - PC - LG Chem

Material Data Center offers the following functions for LUPOY PC 1201-22:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 22 g/10min ASTM D 1238
温度 300 °C -
负载 1.2 kg -
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
拉伸模量 2340 MPa ASTM D 638
屈服应力 60 MPa ASTM D 638
断裂拉伸强度 66 MPa ASTM D 638
屈服伸长率 6 % ASTM D 638
断裂伸长率 120 % ASTM D 638
弯曲模量 2410 MPa ASTM D 790
弯曲强度 96 MPa ASTM D 790
洛克硬度 M 72 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 750 J/m ASTM D 256
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
1.5mm名义厚度时的燃烧性 V-2 class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
灼热丝引燃温度 (GWIT) 850 °C IEC 60695-2-13
GWIT - 测试用试样厚度 2 mm -
ASTM数据
UL94 燃烧性 V-2 - UL 94
测试厚度 0.5 mm -
热释放速率, 平行 68 E-6/K ASTM D 696
DTUL @ 66 psi 142[ann.] °C ASTM D 648
DTUL @ 264 psi 126 °C ASTM D 648
维卡温度 147 °C ASTM D 1525
氧指数 26 % ASTM D 2863
ann.: annealed
电性能价值单位Test Standard
ISO数据
相对漏电起痕指数 250 - IEC 60112
ASTM数据
电介质强度, 短时 17 kV/mm ASTM D 149
耗散因素, 60 Hz 0.001 - ASTM D 150
电介质常数, 60 Hz 3 - ASTM D 150
体积电阻率 2E17 Ohm*cm ASTM D 257
光学特性价值单位Test Standard
ASTM数据
雾度 1.1 % ASTM D 1003
光透射率 89 % ASTM D 1003
折射率 1.59 - ASTM D 542
其它性能价值单位Test Standard
吸水率, 24小时 0.15 % ASTM D 570
吸水率, 平衡 0.32 % ASTM D 570
密度 1200 kg/m³ ASTM D 792
典型数据
加工方法
注塑, 其它挤出成型
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经热稳处理的/耐热的, 透明.
Certifications
可食品接触的, FDA 21 CFR认证
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com