Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S 778T XA SPF60 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S 778T XA SPF60:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Luran® S 778T XA SPF60 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S 778T XA SPF60 is an injection molding grade with enhanced heat resistance, brilliant surface appearance and best UV resistance among all Luran® S products.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 5 cm³/10min ISO 1133
温度 220 °C -
载荷 10 kg -
模塑收缩率, 平行 0.6 % ISO 294-4, 2577
熔体 0.17 W/(m K) -
喷射温度 98 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2500 MPa ISO 527
屈服应力 52 MPa ISO 527
屈服伸长率 3.4 % ISO 527
名义断裂伸长率 8 % ISO 527
简支梁缺口冲击强度, +23°C 15 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 4 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
维卡软化温度, B 103 °C ISO 306
线性热膨胀系数, 平行 90 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
Yellow Card 现存 是的 - -
Other Standards[S]
热导率, 固态 0.17 W/(m K) ISO 22007-4
S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
密度 1070 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 240 - 280 °C -
模具温度 40 - 80 °C -
函数
粘度-剪切速度 , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
剪切应力-剪切速度 , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
动态剪切模量-温度 , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
应力-应变.  , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
正割模量-应变.  , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
应力-应变(等时的) 23°C, Luran® S 778T XA SPF60, ASA, INEOS Styrolution
蠕变模量-时间. 23°C, Luran® S 778T XA SPF60, ASA, INEOS Styrolution
蠕变曲线 23°C, Luran® S 778T XA SPF60, ASA, INEOS Styrolution
应力-应变(等时的) 60°C, Luran® S 778T XA SPF60, ASA, INEOS Styrolution
蠕变模量-时间. 60°C, Luran® S 778T XA SPF60, ASA, INEOS Styrolution
蠕变曲线 60°C, Luran® S 778T XA SPF60, ASA, INEOS Styrolution
比容-温度(pvT) , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
拉伸模量-温度 , Luran® S 778T XA SPF60, ASA, INEOS Styrolution
典型数据
加工方法
注塑
供货形式
粒料, 黑色
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
特征
High Gloss
耐化学试剂
通用耐化学性
应用
汽车
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 240 - 280°C

Mold temperature, range: 40 - 80°C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.