Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S ECO 776SE BC40 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S ECO 776SE BC40:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Luran® S ECO 776SE BC40 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S ECO 776SE BC40 is suitable extrusion applications. It provides good impact toughness and enables matte surface appearance for extruded sheets. Luran® S ECO 776SE BC40 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 53 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 40 %
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 4 cm³/10min ISO 1133
温度 220 °C -
载荷 10 kg -
熔体 0.17 W/(m K) -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2200 MPa ISO 527
屈服应力 47 MPa ISO 527
屈服伸长率 3.3 % ISO 527
名义断裂伸长率 12 % ISO 527
弯曲模量, 23°C 2000 MPa ISO 178
弯曲强度 65 MPa ISO 178
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 30 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 4 kJ/m² ISO 179/1eA
球压硬度 70 MPa ISO 2039-1
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 96 °C ISO 75-1/-2
热变形温度, 0.45 MPa 101 °C ISO 75-1/-2
维卡软化温度, B 92 °C ISO 306
线性热膨胀系数, 平行 95 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 3.0 mm -
燃烧速率, FMVSS, 厚度:1毫米 25[1] mm/min ISO 3795 (FMVSS 302)
燃烧性-氧指数 19 % ISO 4589-1/-2
Other Standards[S]
热导率, 固态 0.17 W/(m K) DIN 52612-1
1: 2 mm  S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
吸水性 1.65 % 类似ISO 62
吸湿性 0.35 % 类似ISO 62
密度 1070 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
加工推荐(挤出)价值单位Test Standard
Type of extrusion profile - -
预干燥-温度 80 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 240 °C -
Type of extrusion sheet - -
预干燥-温度 80 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 210 - 250 °C -
函数
应力-应变.  , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
正割模量-应变.  , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
应力-应变(等时的) 23°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变模量-时间. 23°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变曲线 23°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
应力-应变(等时的) 40°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变模量-时间. 40°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变曲线 40°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
应力-应变(等时的) 60°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变模量-时间. 60°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变曲线 60°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
应力-应变(等时的) 80°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变模量-时间. 80°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
蠕变曲线 80°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
比容-温度(pvT) , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
拉伸模量-温度 , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
典型数据
加工方法
异型材挤出成型, 片材挤出成型, 其它挤出成型, 吹塑, 热成型
供货形式
粒料
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
耐化学试剂
通用耐化学性
Certifications
生物相容, ISCC Plus
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
其E烦龀尚
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Pipes, Melt temperature: 200 - 240°C

E尾募烦龀尚
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Profiles, Melt temperature: 240°C

板材挤出成型
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Plates, Melt temperature: 210 - 250°C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com