材料文字说明
- MVR (300 °C/1.2 kg) 9.0 cm³/10 min
- medical devices
- suitable for ETO and steam sterilization at 121 °C
- biocompatible according to many ISO 10993-1 test requirements
- medium viscosity
- easy release
加工/物理特性 | 价值 | 单位 | Test Standard |
ISO数据 |
熔体体积流动速度, MVR |
9 |
cm³/10min |
ISO 1133 |
温度 |
300 |
°C |
- |
载荷 |
1.2 |
kg |
- |
熔融指数, MFI |
10 |
g/10min |
ISO 1133 |
温度 |
300 |
°C |
- |
负载 |
1.2 |
kg |
- |
模塑收缩率, 平行 |
0.7 |
% |
ISO 294-4, 2577 |
模塑收缩率, 垂直 |
0.8 |
% |
ISO 294-4, 2577 |
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
拉伸模量 |
2400 |
MPa |
ISO 527 |
屈服应力 |
66 |
MPa |
ISO 527 |
屈服伸长率 |
6.1 |
% |
ISO 527 |
名义断裂伸长率 |
>50 |
% |
ISO 527 |
弯曲模量, 23°C |
2400 |
MPa |
ISO 178 |
弯曲强度 |
97 |
MPa |
ISO 178 |
拉伸蠕变模量, 1h |
2200 |
MPa |
ISO 899-1 |
拉伸蠕变模量, 1000h |
1900 |
MPa |
ISO 899-1 |
无缺口简支梁冲击强度, +23°C |
N |
kJ/m² |
ISO 179/1eU |
简支梁缺口冲击强度, +23°C |
75 |
kJ/m² |
ISO 179/1eA |
Type of failure |
P |
- |
- |
简支梁缺口冲击强度, -30°C |
16 |
kJ/m² |
ISO 179/1eA |
Type of failure |
C |
- |
- |
悬臂梁缺口冲击强度, +23°C |
70 |
kJ/m² |
ISO 180/1A |
悬臂梁缺口冲击强度 |
15 |
kJ/m² |
ISO 180/1A |
悬臂梁缺口冲击强度 - 温度 |
-30 |
°C |
- |
冲孔最大力, +23°C |
5400 |
N |
ISO 6603-2 |
冲孔最大力, -30°C |
6300 |
N |
ISO 6603-2 |
冲孔功, +23°C |
60 |
J |
ISO 6603-2 |
冲孔功, -30°C |
65 |
J |
ISO 6603-2 |
球压硬度 |
115 |
MPa |
ISO 2039-1 |
热性能 | 价值 | 单位 | Test Standard |
ISO数据 |
玻璃化转变温度, 10°C/min |
145 |
°C |
ISO 11357-1/-2 |
热变形温度, 1.80 MPa |
125 |
°C |
ISO 75-1/-2 |
热变形温度, 0.45 MPa |
137 |
°C |
ISO 75-1/-2 |
维卡软化温度, B |
145 |
°C |
ISO 306 |
线性热膨胀系数, 平行 |
65 |
E-6/K |
ISO 11359-1/-2 |
线性热膨胀系数, 垂直 |
65 |
E-6/K |
ISO 11359-1/-2 |
厚度为h时的燃烧性 |
V-2 |
class |
IEC 60695-11-10 |
测试用试样的厚度 |
0.8 |
mm |
- |
Yellow Card 现存 |
是的 |
- |
- |
燃烧性-氧指数 |
28 |
% |
ISO 4589-1/-2 |
灼热丝燃烧指数 (GWFI) |
850 |
°C |
IEC 60695-2-12 |
GWFI - 测试用试样厚度 |
1.5 |
mm |
- |
灼热丝燃烧指数 (GWFI) |
930 |
°C |
IEC 60695-2-12 |
GWFI - 测试用试样厚度 |
3 |
mm |
- |
灼热丝引燃温度 (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - 测试用试样厚度 |
0.75 |
mm |
- |
灼热丝引燃温度 (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - 测试用试样厚度 |
1.5 |
mm |
- |
灼热丝引燃温度 (GWIT) |
900 |
°C |
IEC 60695-2-13 |
GWIT - 测试用试样厚度 |
3 |
mm |
- |
Other Standards[S] |
热导率, 固态 |
0.2 |
W/(m K) |
ISO 8302 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
电性能 | 价值 | 单位 | Test Standard |
ISO数据 |
相对介电常数., 100Hz |
3.1 |
- |
IEC 62631-2-1 |
相对介电常数., 1MHz |
3 |
- |
IEC 62631-2-1 |
介质损耗因子, 100Hz |
5 |
E-4 |
IEC 62631-2-1 |
介质损耗因子, 1MHz |
90 |
E-4 |
IEC 62631-2-1 |
体积电阻率 |
>1E13 |
Ohm*m |
IEC 62631-3-1 |
表面电阻率 |
>1E15 |
Ohm |
IEC 62631-3-2 |
介电强度 |
34 |
kV/mm |
IEC 60243-1 |
相对漏电起痕指数 |
250 |
- |
IEC 60112 |
光学特性 | 价值 | 单位 | Test Standard |
ISO Data |
浑浊率 |
0.8 |
- |
ISO 14782 |
光输送 |
89 |
% |
ISO 13468-1, -2 |
Other Standards[S] |
折射率 |
1.59 |
- |
ISO 489 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
其它性能 | 价值 | 单位 | Test Standard |
吸水性 |
0.3 |
% |
类似ISO 62 |
吸湿性 |
0.12 |
% |
类似ISO 62 |
密度 |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
660 |
kg/m³ |
- |
试样制备条件 | 价值 | 单位 | Test Standard |
ISO数据 |
注塑, 熔体温度 |
300 |
°C |
ISO 294 |
注塑, 模具温度 |
80 |
°C |
ISO 294 |
注塑, 注射速度 |
200 |
mm/s |
ISO 294 |
加工推荐(注塑) | 价值 | 单位 | Test Standard |
预干燥-温度 |
120 |
°C |
- |
预干燥-时间 |
2 - 3 |
h |
- |
加工湿度 |
≤0.02 |
% |
- |
注塑熔体温度 |
280 - 320 |
°C |
- |
模具温度 |
80 - 120 |
°C |
- |
1区 |
250 - 260 |
°C |
- |
2区 |
270 - 280 |
°C |
- |
3区 |
280 - 290 |
°C |
- |
喷嘴温度 |
290 - 300 |
°C |
- |
背压 |
5 - 15 |
MPa |
- |
典型数据
加工方法
注塑
供货形式
粒料
添加剂
脱模助剂
特殊性能
透明., Opaque, 消毒, 环氧乙烷灭菌(EtO), 蒸汽灭菌
Certifications
生物相容, 回收树脂含量, 医用级, Biocompatibility ISO 10993, ISCC Plus
应用
药物
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com