Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® E3TZ - ABS - INEOS Styrolution

Material Data Center offers the following functions for Novodur® E3TZ:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Novodur® E3TZ acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® E3TZ is an extrusion grade with high gloss and good surface appearance. It is optimized for processing via thermoforming. Furthermore, food contact statements are available upon request.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 8 cm³/10min ISO 1133
温度 220 °C -
载荷 10 kg -
模塑收缩率, 平行 0.6 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 2550 MPa ISO 527
屈服应力 48 MPa ISO 527
屈服伸长率 2.5 % ISO 527
名义断裂伸长率 15 % ISO 527
弯曲模量, 23°C 2600 MPa ISO 178
弯曲强度 75 MPa ISO 178
无缺口简支梁冲击强度, +23°C 150 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 110 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 19 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 9 kJ/m² ISO 179/1eA
球压硬度 110 MPa ISO 2039-1
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 98 °C ISO 75-1/-2
热变形温度, 0.45 MPa 103 °C ISO 75-1/-2
维卡软化温度, B 100 °C ISO 306
线性热膨胀系数, 平行 90 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
灼热丝燃烧指数 (GWFI) 700 °C IEC 60695-2-12
GWFI - 测试用试样厚度 2 mm -
电性能价值单位Test Standard
ISO数据
表面电阻率 600 Ohm IEC 62631-3-2
介电强度 35 kV/mm IEC 60243-1
其它性能价值单位Test Standard
密度 1050 kg/m³ ISO 1183
加工推荐(挤出)价值单位Test Standard
Type of extrusion profile - -
预干燥-温度 80 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 215 - 240 °C -
Type of extrusion sheet - -
预干燥-温度 80 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 215 - 240 °C -
典型数据
加工方法
异型材挤出成型, 片材挤出成型, 其它挤出成型, 热成型
供货形式
粒料
特殊性能
高冲击韧性的/经抗冲改性的
特征
High Gloss
Certifications
可食品接触的
地区供应
欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
E尾募烦龀尚
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Profiles, Melt temperature: 215 - 240°C

板材挤出成型
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Sheets, Melt temperature: 215 - 240°C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.