Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Nypel® 6235G BK1 - PA6-GF35 - BASF

Material Data Center offers the following functions for Nypel® 6235G BK1:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Nypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Nypel 6235G BK1 is a 35% glass reinforced injection molding grade of PA6. Based on recycled polyamide feedstocks, Nypel 6235G BK1 offers a balance of mechanical properties with excellent flow and surface appearance.

Nypel 6235G BK1 is recommended for lawn and power equipment housings, structural furniture components such as seat frames, and automotive and industrial applications.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 76 / * cm³/10min ISO 1133
温度 275 / * °C -
载荷 5 / * kg -
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 10999 / 7854 MPa ISO 527
断裂应力 172 / 116 MPa ISO 527
断裂伸长率 3.2 / 6.2 % ISO 527
无缺口简支梁冲击强度, +23°C 90 / 104 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 77 / 75 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 17 / 20 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 14 / 14 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 218 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 207 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 217 / * °C ISO 75-1/-2
其它性能干 / 已调节单位Test Standard
吸水性 1.25 / * % 类似ISO 62
吸湿性 5.1 / * % 类似ISO 62
密度 1380 / - kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 4 h -
注塑熔体温度 270 - 290 °C -
模具温度 80 - 90 °C -
典型数据
加工方法
注塑
供货形式
黑色
Certifications
回收树脂含量
应用
汽车
地区供应
北美
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.