Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of P84®NT2 HCM - PI - Evonik Operations GmbH

Material Data Center offers the following functions for P84®NT2 HCM:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other P84 datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Neat aromatic Polyimide

Polyimid P84® NT - at a glance

 

  • Excellent performance at high temperatures
  • High strength and excellent shape stability
  • Very good impact resistance
  • High heat deflection temperature
  • Very good creep resistance even at elevated temperatures
  • Machinable with standard tools
  • Low wear and friction behaviour
  • Processing by Hot compression molding

 

 

Application examples

bushings, seals, bearings components, guides, gear wheels, and valve parts

in the automotive and aerospace industries and in industrial equipment.

For further information please visit WWW.P84.COM.

机械性能价值单位Test Standard
ISO数据
拉伸模量 3428 MPa ISO 527
断裂应力 132 MPa ISO 527
断裂伸长率 6.3 % ISO 527
无缺口简支梁冲击强度, +23°C 133 kJ/m² ISO 179/1eU
Type of failure C - -
简支梁缺口冲击强度, +23°C 7.5 kJ/m² ISO 179/1eA
Type of failure C - -
肖氏硬度D 88 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 364 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 340 °C ISO 75-1/-2
热变形温度, 0.45 MPa 377 °C ISO 75-1/-2
线性热膨胀系数, 平行 36 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 37 kV/mm IEC 60243-1
相对漏电起痕指数 125 - IEC 60112
其它性能价值单位Test Standard
密度 1380 kg/m³ ISO 1183
典型数据
加工方法
模压成型
供货形式
粒料, 碎粒料, 粉料
特殊性能
高冲击韧性的/经抗冲改性的, 经热稳处理的/耐热的
特征
防蠕变, Tribologic Grade
应用
航天航空, 汽车
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.