Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 5533 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 5533 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Polyether block amide Pebax® 5533 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SP grade has been developed to be heat and UV resistant.


Main applications:
  • Athletic foot wear components
  • Ski shoes
  • High performance power trasmission belts


Packaging:

This grade is delivered dried in sealed packaging (20 or 25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 170 / 161 MPa ISO 527
屈服应力 12 / 12 MPa ISO 527
屈服伸长率 25 / 25 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
10%应变时的应力 10 / * MPa ISO 527
100%应变时的应力 14 / * MPa ISO 527
断裂应力 TPE 52 / * MPa ISO 527
断裂应变 TPE >300 / * % ISO 527
23°C时恒定应变下的永久变形, 24h 43 / * % ISO 815
撕裂强度 106 / * kN/m ISO 34-1
耐磨性 47 / * mm³ ISO 4649
肖氏硬度D 50 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 159 / * °C ISO 11357-1/-3
热变形温度, 0.45 MPa 66 / * °C ISO 75-1/-2
维卡软化温度, B 66 / * °C ISO 306
线性热膨胀系数, 平行 170 / * E-6/K ISO 11359-1/-2
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 9 / - - IEC 62631-2-1
相对介电常数., 1MHz 5 / - - IEC 62631-2-1
介质损耗因子, 100Hz 1110 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 1020 / - E-4 IEC 62631-2-1
体积电阻率 3.2E11 / - Ohm*m IEC 62631-3-1
表面电阻率 * / 3E12 Ohm IEC 62631-3-2
介电强度 38.5 / - kV/mm IEC 60243-1
相对漏电起痕指数 * / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.2 / * % 类似ISO 62
吸湿性 0.6 / * % 类似ISO 62
密度 1010 / 1010 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 65 - 75 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 200 - 270 °C -
模具温度 25 - 60 °C -
函数
粘度-剪切速度 , Pebax® 5533 SP 01, TPA, ARKEMA
剪切应力-剪切速度 , Pebax® 5533 SP 01, TPA, ARKEMA
应力-应变.  , Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
应力-应变.  , Pebax® 5533 SP 01 (状况), TPA, ARKEMA
正割模量-应变.  , Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
正割模量-应变.  , Pebax® 5533 SP 01 (状况), TPA, ARKEMA
应力-应变(等时的) 23°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变模量-时间. 23°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变曲线 23°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
应力-应变(等时的) 40°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变模量-时间. 40°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变曲线 40°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
应力-应变(等时的) 60°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变模量-时间. 60°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变曲线 60°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
应力-应变(等时的) 80°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变模量-时间. 80°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
蠕变曲线 80°C, Pebax® 5533 SP 01 (烘干), TPA, ARKEMA
比容-温度(pvT) , Pebax® 5533 SP 01, TPA, ARKEMA
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 其它挤出成型, 模压/烧结成型, 浇铸成型, 热成型
供货形式
粒料
特殊性能
可电镀的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
其他信息
注塑成型

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 200°C / 240°C / 270°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
其E烦龀尚

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 220°C / 230°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.