Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 7433 SA 01 MED - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 7433 SA 01 MED:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Polyether block amide 7433 SA 01 MED resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices.
Pebax® 7433 SA 01 MED resin also offers an excellent combination of properties such as: kink resistance, low friction coefficient and superior dynamic response.
Upon request, letters regarding USP Class VI compliance can be provided.


Main applications:
  • Tubings like angiography and angioplasty catheters
  • Flexible injected parts


Packaging:

This grade is delivered dried in sealed packaging (20 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 - / 700 MPa ISO 527
屈服应力 - / 30 MPa ISO 527
屈服伸长率 - / 17 % ISO 527
名义断裂伸长率 - / >50 % ISO 527
简支梁缺口冲击强度, +23°C - / 19 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C - / 6 kJ/m² ISO 179/1eA
断裂应力 TPE 46 / * MPa ISO 527
耐磨性 40.5 / * mm³ ISO 4649
肖氏硬度D 66 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 174 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 67 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 113 / * °C ISO 75-1/-2
维卡软化温度, B 129 / * °C ISO 306
其它性能干 / 已调节单位Test Standard
吸水性 1.43 / * % 类似ISO 62
吸湿性 0.76 / * % 类似ISO 62
密度 1010 / - kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 70 - 80 °C -
预干燥-时间 5 - 7 h -
注塑熔体温度 230 - 290 °C -
模具温度 25 - 60 °C -
典型数据
加工方法
注塑, 其它挤出成型
供货形式
粒料
特殊性能
经光稳处理的/耐光的, 经热稳处理的/耐热的
Certifications
医用级, US药物六级认证
地区供应
其他信息
注塑成型

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 260°C / 290°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 5-7 hours at 70-80°C.
其E烦龀尚

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 220°C / 235°C / 250°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 5-7 hours at 70-80°C.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.